Study on Behaviour of Flexural Members by Elastic Approach

DOI : 10.17577/IJERTV5IS070309

Download Full-Text PDF Cite this Publication

  • Open Access
  • Total Downloads : 172
  • Authors : Miss. Priyanka Asutkar, Dr. S. B. Shinde, P. R. Punase
  • Paper ID : IJERTV5IS070309
  • Volume & Issue : Volume 05, Issue 07 (July 2016)
  • DOI : http://dx.doi.org/10.17577/IJERTV5IS070309
  • Published (First Online): 22-07-2016
  • ISSN (Online) : 2278-0181
  • Publisher Name : IJERT
  • License: Creative Commons License This work is licensed under a Creative Commons Attribution 4.0 International License

Text Only Version

Study on Behaviour of Flexural Members by Elastic Approach

Priyanka Asutkar Dr. S. B. Shinde P. R. Punase

PG Student Head of Civil Department Assistant Professor

MGMS JNEC MGMS JNEC SSBT Collage of Engineering

Aurangabad, MH, India Aurangabad, MH, India Bambhori, Jalgaon,MH,India

Abstract: Concrete is one the most extensively used construction material all over the world. Many scientists and researchers are in quest for developing alternate construction material that are environment friendly and contribute towards sustainable development. Huge amount of rubber tyres waste is being generating day by day which creates the disposal problem and has many environmental issues. As this scrap rubber waste is an elastic material having less specific gravity, energy absorbent material can be used as a replacement material for obtaining light weight concrete. In present study the modified concrete is prepared by replacing coarse aggregates in concrete with rubber aggregates by varying the replacement proportion from 0% to 20% with increment of 5%. The elastic properties are determined from concrete cubes. 3 cubes for each percentage of replacement are casted and tested after 28th days of curing. Method of initial functions is used for the analysis of beams. The Method of initial functions (MIF) is an analytical method of elasticity theory from which stresses and displacement can be determined. This attempt of replacing the coarse aggregates with rubber aggregates will save the natural aggregates, reduces weight of structure and also helps achieve sustainability.

Key words: Rubber scrap, elasticity, Method of initial functions, beams.

    1. INTRODUCTION

      The scarcity and availability of sand and aggregate at reasonable rates are now giving anxiety to the construction industry. Over years, deforestation and extraction of natural aggregates from river beds, lakes and other water bodies have resulted in huge environmental problems. Erosion of the existing topography usually results in flooding and landslides. Moreover, the filtration of rain water achieved by deposits of natural sand is being lost, thereby causing contamination of water reserves used for human consumption. Hence, to prevent pollution authorities are imposing more and more stringent restrictions on the extraction of natural aggregates and its crushing. The best way to overcome this problem is to find alternate aggregates for construction in place of conventional natural aggregates. In this research rubber aggregates from discarded tyre rubber in sizes 20-10 mm, is partially replaced with natural aggregates in cement concrete.

    2. Method of initial functions (MIF)

MIF was first proposed by Malieev in 1951 and further developed by Vlasov in 1955. Beams that are built of more than one material are called comp-osite beams. It is difficult to analyze the laminated beams by the bending theory used for ordinary beams. In MIF, equations

governing the flexure of composite laminated beams are derived without making any assumption regarding the physical behaviour of beams. The method of initial functions (MIF) has been used for deriving the equations. It is an analytical method of elasticity theory allows us to obtain the exact solutions for certain types of problems without use of hypotheses about the charac-ter of the stress-strain state of the structural element. In recent years the MIF has been used intensively for the analysis of various problems. For example, three-dimensional elasticity equations for circular cylind-rical shells are solved by assuming Taylor series expansions for finding stresses and displacements.

2.0 LITERATURE REVIEW

Recycled tire rubber is used to develop deliberately low elastic modulus and highly ductile ECC repair material so as to alleviate repair failure induced by restrained drying shrinkage [1].Tyre aggregate replaced with coarse aggregate with various percentages and compared with regular concrete. Fresh and hardened concrete strength were identified [2].Rubber waste additives reduced both static and dynamic modulus of elasticity [3].Higher content of waste tyre crumb rubber particle used in concrete increases workability of concrete and produce the light weight concrete [4].Compressive strength of concrete with 100% replacement of chipped rubber showed 90% reduction. However reduction in strength was 80% when crumb rubber was used as 100% replacement to sand in concrete [5].The replacement of coarse aggregate by junk rubber in concrete has resulted in reduced compressive strength and densities [6].Rubber tyre aggregate were added to M35 mix with different percentages. Gradual reduction in the compressive and tensile strength was observed. Upto 8% of rubber aggregate can be added in the concrete without considerable reduction in strength [7].Replacement of rubber increased water permeability depth in the concrete and increases the water absorption in case of coarse aggregate replacement but reduces the water absorption in case of cement replacement. [8].Slump value is decreased as the percentage of replacement of scrap tyre rubber increase so decrease in workability. Also decrease in compressive, split tensile and flexural strength. In the rubberized concrete the loss of strength was 45% with 15% replacement of coarse aggregate with rubber particle [9]. Replacing conventional fine aggregate with crumb rubber at 1030%, the unit-weight of concrete can be reduced from 14%up to 28% depending on the type and the content of the crumb rubber. The CR concrete exhibits superior thermal and

sound properties than plain concrete as measured by the decrease in thermal conductivity coefficient, increase in sound absorption coefficient and noise reduction coefficient [10].Method of initial functions is used for two dimensional elasto dynamic problems for plain stress and plain strain conditions [11]. Method of initial function is used for the study of composite beams having two layers of orthotropic material and developed governing equation [13].Result obtained with MIF are compared with result obtained by FEM based software ANSYS and it is observed that they are comparable [14].MIF is successfully applied for the analysis of reinforced concrete brick layer [15]The method of initial function is used to see the effect of elastic properties on the behaviour of the beam [16].The deflection obtained by MIF is equal to the deflection obtained by other theories. The normal stress equal to the intensity of loading and shear stress equal to zero at the top of beam are obtain, this shows that MIF is successfully applied for the analysis of beam [17].MIF gives correct result for both shallow and deep beams. Also in this method it is not necessary to assume the position of neutral axis; it incorporates the position of neutral axis by itself. Hence it is conclude that analysis done by MIF provides more realistic behaviour of beam sections of any depth [18].

Fig 1. Rubber Aggregates (20mm)

    1. MATERIAL AND METHODS

      The rubber aggregates are obtained by shredding the scrap tire rubber in 20mm size. Heavy vehicles tire scraps were used for preparing the rubber aggregates. The percentage of replacement is done by volume. Cubes size is taken as 150 x1 50 x 150 mm. The properties of material used are discussed below.

      Table 1: Physical properties of materials used

      Material

      Specific gravity

      Bulk Density (kg/m3)

      Rubber aggregates

      1.10

      650

      Fine aggregates

      2.6

      <>1650

      Coarse aggregates

      2.8

      1720

      Designation

      Cement (kg)

      Water (litres)

      Fine aggregates (kg)

      Coarse aggregates (kg)

      Rubber aggregates (kg)

      NC – 0%

      364.81

      225.17

      610.43

      1239.64

      RC -5%

      437.77

      224.2

      590.03

      1177.65

      23.30

      RC -10%

      437.77

      224.2

      590.03

      1115.67

      46.73

      RC- 15%

      437.77

      224.2

      590.03

      1053.69

      70.101

      RC-20%

      437.77

      224.2

      590.03

      991.71

      93.46

      Designation

      Cement (kg)

      Water (litres)

      Fine aggregates (kg)

      Coarse aggregates (kg)

      Rubber aggregates (kg)

      NC – 0%

      364.81

      225.17

      610.43

      1239.64

      RC -5%

      437.77

      224.2

      590.03

      1177.65

      23.30

      RC -10%

      437.77

      224.2

      590.03

      1115.67

      46.73

      RC- 15%

      437.77

      224.2

      590.03

      1053.69

      70.101

      RC-20%

      437.77

      224.2

      590.03

      991.71

      93.46

      Table 2. Mix proportion (kg/m3)

      Fig 2. Concrete Cubes

    2. Compressive test on concrete cubes

The coarse aggregates in the concrete was replaced successively by different percentage of rubber aggregates with varying proportion from 0%, 5%, 10%, 15%, 20%.The concrete cubes of size 150mm3 were casted and tested after 28 days of curing.

Fig 3. Testing of concrete cubes

Table 3. Compressive strength of cubes for various percentage of replacement

% of replacement

coarse aggregates replaced concrete (N/mm2)

0%

31.7

5%

29.23

10%

25.61

15%

21.34

20%

16.61

4. ANALYSIS OF COMPOSITE BEAM BY MIF

The following values of beam dimensions are chosen for the particular problem.

H=250mm, l=2000mm.

The boundary condition of simply supported edges is given by

X=Y=v=0, at x=0 and x=l

A uniformly distributed load is assumed, on top surface of the beam. The expression for point load in sine series is given by

P 4Po {sin( x )}

l l

Fig 4. Variation of compressive strength for different percentage of replacement

Taking Po=100 N/m and x=l/2.

The design loads Po are calculated by using IS 456- 2000. The elastic properties are determined by using expression from ACI-318. is constant for all cases, and G is determined by using the expression E=2G(1+ ).

Table 4. Elastic Properties

Material

% of Replacement of Coarse Aggregates

Load (N/mm)

E

(N/mm2)

G

(N/mm2)

Coarse Aggregates Replaced with Rubber aggregates Concrete

0

100

28729.13

1197.47

0.20

5

98.80

24658.06

10274.19

0.20

10

97.50

21589.82

8995.75

0.20

15

93.20

16827.65

7011.52

0.20

20

85.20

14284.55

5951.89

0.20

4.1 Results and Discussion

The analytical results of stresses and displacement by using method of initial functions are shown in the following table.

Table 7. Beam loaded with point load 97.50 KN

Depth of Beam

v (mm)

X

(N/mm2)

Bending stress (N/mm2)

400

0.641

6.84

7.130

350

0.641

5.13

5.290

300

0.641

3.5

3.580

250

0.641

1.94

1.510

200

0.640

0.15

0.710

150

0.639

-1.06

-1.127

100

0.638

-2.56

-2.743

50

0.636

-4.08

-4.308

0

0.634

0

-5.964

Depth of Beam

v (mm)

X

(N/mm2)

Bending stress (N/mm2)

400

0.641

6.84

7.130

350

0.641

5.13

5.290

300

0.641

3.5

3.580

250

0.641

1.94

1.510

200

0.640

0.15

0.710

150

0.639

-1.06

-1.127

100

0.638

-2.56

-2.743

50

0.636

-4.08

-4.308

0

0.634

0

-5.964

Table 5. Beam loaded with UDL100N/mm.

Depth Of Beam

V (mm)

X (N/mm2)

Bending Stress (N/mm2)

400

0.513

0

7.31

350

0.513

0.53

5.43

300

0.513

0.78

3.661

250

0.513

0.93

1.957

200

0.512

0.968

0.30

150

0.511

0.92

-1.331

100

0.511

0.79

-2.966

50

0.509

0.54

-4.628

0

0.507

0

-6.352

Depth Of Beam

V (mm)

X (N/mm2)

Bending Stress (N/mm2)

400

0.513

0

7.31

350

0.513

0.53

5.43

300

0.513

0.78

3.661

250

0.513

0.93

1.957

200

0.512

0.968

0.30

150

0.511

0.92

-1.331

100

0.511

0.79

-2.966

50

0.509

0.54

-4.628

0

0.507

0

-6.352

Depth of Beam

v (mm)

X

(N/mm2)

Bending stress (N/mm2)

400

0.734

0

6.990

350

0.7.33

0.35

5.242

300

0.733

0.62

3.495

250

0.732

0.78

1.380

200

0.732

0.85

0.120

150

0.730

0.81

-1.033

100

0.728

0.66

-2.262

50

0.728

0.39

-3.850

0

0.725

0

-5.321

Depth of Beam

v (mm)

X

(N/mm2)

Bending stress (N/mm2)

400

0.734

0

6.990

350

0.7.33

0.35

5.242

300

0.733

0.62

3.495

250

0.732

0.78

1.380

200

0.732

0.85

0.120

150

0.730

0.81

-1.033

100

0.728

0.66

-2.262

50

0.728

0.39

-3.850

0

0.725

0

-5.321

Table 8. Beam loaded with point load 93.20 KN

Table 6. Beam loaded with point load 98.80 KN

Depth of Beam

v (mm)

X

(N/mm2)

Bending stress (N/mm2)

400

0.581

0

7.220

350

0.581

0.38

5.380

300

0.581

0.67

3.650

250

0.580

0.85

1.928

200

0.580

0.93

0.28

150

0.579

0.88

-1.245

100

0.578

0.73

-2.863

50

0.576

0.43

-4.515

0

0.576

0

-6.233

Table 8. Beam loaded with point load 85.50 KN

Depth of Beam

v (mm)

X

(N/mm2)

Bending stress (N/mm2)

400

0.811

0

6.046

350

0.811

0.34

4.533

300

0.810

0.6

3.098

250

0.810

0.76

1.15

200

0.810

0.83

0.095

150

0.810

0.79

-0.939

100

0.807

0.64

-2.153

50

0.807

0.38

-3.607

0

0.805

0

-4.903

The following figure shows the profile of stresses and displacement across the depth of beam.

Fig 5. Variation of bending stress for different percentage of replacement. The bending Stress decreases as the percentage replacement of coarse aggregates by rubber aggregates in concrete increases. Reduction of bending stress is less upto 15% but suddenly decreases by 12% for 20% replacement of coarse aggregates.

Fig 6. Variation of shear stress for different percentage of replacement across the depth. The shear Stress is zero at top end of the beams and maximum at centre. As percentage replacement of coarse aggregates by rubber aggregates in concrete increases the shear stress decreases.

Fig 7. Variation of displacement across depth of beam for different percentage of replacement.

The variation of displacement (v) is almost linear across the depth. It increases with increase in percentage replacement of coarse aggregates by rubber aggregates in concrete. Less variation is observed 5% and 10% but displacement is more for 15 % and 20% replacement

5. CONCLUSIONS

  • The following conclusions are made based on the above experimental work and analysis by MIF.

  • Experimentally it is seen that the compressive strength of the concrete decreases when coarse aggregates are replaced by rubber aggregates. The rubber aggregates can be effectively replaced up to 15%.

  • The results of shear stress and bending stresses are analysed by using MIF satisfies the physical behaviour of beam.

  • The analytical results shows that the bending Stress decreases as the percentage replacement of coarse aggregates by rubber aggregates in concrete increases.

  • The results indicate that displacements are more for rubber aggregates replacement.

  • This study suggest that use of scrap material will help to recycle the material and can be effectively used in concrete. This will save the natural aggregates and also helps to achieves sustainability

REFRENCES

  1. Xiaoyan Huang, Ravi Ranad, Wen Ni, Victor C. Li On the use of recycled tire rubber to develop low E-modulus ECC for durable concrete repairs, Construction and Building Materials 46 (2013) 134141.

  2. Kotresh K.M, Mesfin Getahum Belachew Study On Waste Tyre Rubber As Concrete Aggregates

  3. International Journal of Scientific Engineering and technology,3(4), 2014,433-436.

  4. Gintauta Skripkiunas, Audriud Grinys, Benjaminas Cernius Deformation properties of concrete with Rubber waste additives, Material Science, 13(3),2007, 219-223.

  5. M. R. Wakchaure, Prashant A. Chavan Waste Tyre Crumb Rubber Particle as A Partial Replacement to Fine Aggregate in Concrete, International Journal of Engineering Research & Technology (IJERT), 3(6), 2014, 1206-1209.

  6. El-Gammal, A.; A. K. Abdel-Gawad; Y. El-Sherbini, A. Shalaby Compressive Strength of Concrete Utilizing Waste Tire Rubber, Journal of Emerging Trends in Engineering and Applied Sciences (JETEAS) 1 (1), 96-99.

  7. B.Damodhara Reddy, S.Aruna Jyothy,P,

  8. P. Ramesh Babu Experimental Investigation on Concrete by Partially Replacement of Ware Aggregate with Junk Rubber, The International Journal Of Engineering And Science (IJES), 2(12),2013, 61-65.

  9. Eldhose C., Dr. Soosan T. G. Studies on Scrap Tyre Added Concrete for Rigid Pavements, International Journal of Engineering Research 3(12),2014, 777-779.

  10. Eshmaiel Ganjia, Morteza Khorami, Ali Akbar Maghsoudi Scrap-tyre-rubbr replacement for aggregate and filler in concrete, Construction and Building Materials 23 (2009) 18281836.

  11. K. C. Panda,P. S. Parthi, T. Jena Scrap-Tyre-Rubber Replacement for Aggregate in Cement Concrete: Experimental Study, International Journal of Earth Science and Engineering05,06(01),2012,1692-1701.

  12. Piti Sukontasukkul Use of crumb rubber to improve thermal and sound properties of pre-cast concrete panel Construction and Building Materials 23 (2009) 10841092.

  13. K. T. S. Iyengar, S. K. Pandya, Application of the method of initial functions for the analysis of composite laminated plates, Ingenieur-Arehiv 56,1986,407-416.

  14. Sebastian V.K, Iyengar Raja K.T. and Chandrashekhara K., Method of initial functions in the analysis of thick circular plates, Nuclear Engineering and Design, 36(3), 1976, 341-354.

  15. S.M.Galileev, A.V.Matrosov Method of initial function in the computation of sandwich plate, International Applied Mechanics 31(6), 1995, 496-476.

  16. Sergey M. Galileev, Pavel Y. Tabakov, Mathematical Foundations of the Method of Initial Functions for the Application to Anisotropic Plates, 2nd International Conference on Mechanical, Nanotechnology and Cryogenics Engineering 2013, 59-63.

  17. Patel Rakesh, Dubey S. K, Pathak K.K. Analysis of Composite Beams using Method of Initial Functions, International Journal of Advanced Structures and Geotechnical Engineering, 1(2),2012,83-86.

  18. Patel Rakesh, Dubey S. K, Pathak K.K. Method of Initial Functions for Composite Laminated Beams, International Conference on Benchmarks in Engineering Science and Technology ICBEST, 2012,4-7.

  19. Patel Rakesh, Dubey S. K, Pathak K.K. Analysis of infilled beam using method of initial functions and comparison with FEM, Engineering Science and Technology, an International Journal 17,2014,158-164.